Product specification
13
14
General Purpose
NP0
16 V to 50 V
Surface-Mount Ceramic Multilayer Capacitors
TEST
TEST METHOD
PROCEDURE
REQUIREMENTS
Damp heat
with Ur load
IEC 60384-
21/22
4.13
No visual damage after recovery
1. Preconditioning, class 2 only:
150 +0/-10 °C /1 hour, then keep for
24 ±1 hour at room temp
<General purpose series>
∆C/C
2. Initial measure:
Spec: refer to initial spec C, D, IR
Class 1:
NP0: within ±2% or 1 pF
whichever is greater
3. Damp heat test:
500 ±12 hours at 40 ±2 °C;
90 to 95% R.H. 1.0 Ur applied
D.F.
4. Recovery:
Class 1:
Class 1: 6 to 24 hours
NP0: ≤ 2 x specified value
5. Final measure: C, D, IR
Rins
Class 1:
P.S. If the capacitance value is less than the minimum value
permitted, then after the other measurements have been
made the capacitor shall be preconditioned according to
“IEC 60384 4.1” and then the requirement shall be met.
NP0: ≥ 2,500 MΩ or Rins x Cr ≥ 25s
whichever is less
Endurance
4.14
No visual damage
1. Preconditioning, class 2 only:
150 +0/-10 °C /1 hour, then keep for
24 ±1 hour at room temp
<General purpose series>
∆C/C
2. Initial measure:
Spec: refer to initial spec C, D, IR
Class1:
NP0: within ±2% or 1 pF
whichever is greater
3. Endurance test:
Temperature: NP0: 125 °C
Specified stress voltage applied for 1,000 hours:
Applied 2.0 x Ur for general product.
D.F.
Class1:
4. Recovery time: 24 ±2 hours
5. Final measure: C, D, IR
NP0: ≤ 2 x specified value
Rins
Class1:
P.S. If the capacitance value is less than the minimum value
permitted, then after the other measurements have been
made the capacitor shall be preconditioned according to
“IEC 60384 4.1” and then the requirement shall be met.
NP0: ≥ 4,000 MΩ or Rins x Cr ≥ 40s
whichever is less
Voltage proof
IEC 60384-1 4.6
Specified stress voltage applied for 1 minute
No breakdown or flashover
Ur ≤ 100 V: series applied 2.5 Ur
100 V < Ur ≤ 200 V series applied (1.5 Ur + 100)
200 V < Ur ≤ 500 V series applied (1.3 Ur + 100)
Ur > 500 V: 1.3 Ur
I: 7.5 mA
www.yageo.com
Nov. 24, 2016 V.15